Sign In | Join Free | My rc363.com
China BLOOM(suzhou) Materials Co.,Ltd logo
BLOOM(suzhou) Materials Co.,Ltd
BLOOM(SUZHOU) MATERIALS CO.,LTD Attitude Is Everything.Details Determine Success or Failure.
Verified Supplier

7 Years

Home > Inconel Nickel Alloy >

Stainless Steel Inconel 625 Bar With Stress Corrosion Cracking Resistance

BLOOM(suzhou) Materials Co.,Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now
BLOOM(suzhou) Materials Co.,Ltd
Visit Website
Province/State: Jiangsu
Country/Region: China

Stainless Steel Inconel 625 Bar With Stress Corrosion Cracking Resistance

Stainless Steel Inconel 625 Bar With Stress Corrosion Cracking Resistance

Stainless Steel inconel 625 Ball/Bar Used in Industrial Filed 1 . Descriptions: Nickel Alloy 625 bar, rod, and wire is used for its high strength, easy fabrication (including joining), and outstandin...

Product Tags:

inconel 625 material

      

inconel 718 material

      
Send your message to this supplier
 
*From:
*To: BLOOM(suzhou) Materials Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)